Uniformity Labs launches low-porosity UniJet SS17-4PH stainless steel for Desktop Metal Production System

MaterialsNews
June 15, 2023
Uniformity Labs has released a low-porosity 17-4PH stainless steel powder compatible with the Desktop Metal Production System (Courtesy Desktop Metal)
Uniformity Labs has released a low-porosity 17-4PH stainless steel powder compatible with the Desktop Metal Production System (Courtesy Desktop Metal)

Uniformity Labs, Fremont, California, USA, has announced the availability of its ultra-low porosity 17-4PH stainless steel powder jet UniJet™ SS17-4PH Performance for the Desktop Metal Production System. The qualified powder is reported to deliver double the green strength of existing stainless steel powders, due to its uniform powder bed layering.

UniJet 17-4PH is also reported to result in an average of 20% less shrinkage than other stainless steel powders qualified for use on the Desktop Metal machine. These factors are said to result in better-sintered part geometric accuracy and less breakage of green and brown parts during post-build handling and depowdering, resulting in high process yield at high throughput.

“The application of Uniformity UniJet 17-4 PH stainless steel for BJT delivers mechanical and process excellence for our customers who require materials that perform to the highest standards across each step of the production process,” said Adam Hopkin, Uniformity founder and CEO. “Our powders deliver superior mechanical properties, printing yield, and process stability, delivering repeatable production scale Binder Jetting.”

One advantage noted by the company is the improved apparent and tapped densities of UniJet 17-4PH, resulting in green parts with more contact points between particles and higher density (10% reduction in relative porosity) than standard Binder Jetting powders. This enables green parts with reportedly twice the magnitude of transverse rupture strength across all layer thicknesses. Such green parts, alongside the very high flowability of Uniformity powder, result in the fabrication of more complex thin-walled or heavier green parts with larger aspect ratios viable by minimising breakage during the de-powdering of large, high aspect ratio and geometrically complex parts with fine features and channels.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Uniformity’s UniJet 17-4PH powder on the Production System is said to have consistently achieved about 25% less shrinkage in X, 19% less shrinkage in Y, and almost 20% less shrinkage in Z axes than the standard Binder Jetting powder across all layer thicknesses. The powder repeatably delivers 99-100% final part density. UniJetTM 17-4PH powder yielded parts with, on average, three-times lower standard deviation in green density than standard binder jetting powder.

The highly flowable powder is said to improve throughput by allowing repeatable fast layering at thicker layers. At 75 µm layer thickness and with 20% reduced shrinkage (allowing more parts fit on the bed), a net throughput benefit of approximately 25% relative to standard Binder Jetting powders for the Desktop Metal machine enables further cost reduction for parts manufacturers. At 110 µm layer thickness – still delivering improvements in green strength, uniformity of powder bed, and sintered density relative to standard inert gas atomised Binder Jetting powders printing at 65 µm layer thickness – the throughput improvement is over 80%.

“Desktop Metal is delighted to offer this highly advanced 17-4 PH stainless steel powder from Uniformity Labs for our Production System platform,” added Ric Fulop, founder and CEO of Desktop Metal. “This latest addition to our material portfolio allows us to binder jet 17-4 PH stainless steel materials critical to producing complex designs. Binder Jetting powders processed with Uniformity Labs technology enables unmatched mechanical properties and can further improve the economics of printing. We look forward to continuing to collaborate with the Uniformity team.”

Shri Shetty, CEO of Zeda and a partner of Uniformity Labs, stated, “This is not the first time we’ve partnered together to develop materials, and Uniformity’s powders have a history of exhibiting superior mechanical properties and higher machine productivity, which will help us further our mission to build things better together in the medical device industry.”

www.uniformitylabs.com

www.desktopmetal.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
June 15, 2023

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap