Mantle showcases growing adoption of AM in injection moulding

ApplicationsNews
February 20, 2023
H13 inserts from Nicolet Plastics (Courtesy Mantle)
H13 inserts from Nicolet Plastics (Courtesy Mantle)

Mantle, San Francisco, California, USA, has highlighted two recent injection moulding customers which have successfully adopted its technology to automate their toolmaking processes. Nicolet Plastics and Westec Plastics both serve the medical device market and will implement Mantle’s technology to reduce the time and labour required to make precise injection mould tooling components.

“As an injection moulder, Mantle allows us to bring additional tool production in-house and increase the complexity of the tools and inserts we manufacture. We will significantly reduce the time it takes to produce production-quality tools and be able to start production in weeks versus months,” stated Tony Cavalco, CEO, Nicolet Plastics CEO.

Mantle uses its proprietary TrueShape technology – a hybrid material extrusion (MEX), CNC and sinter-based process. The system includes its P-200 Additive Manufacturing machine, built on a CNC platform, that integrates building and machining to produce parts with the accuracy and surface finish required for tooling. The P-200 machine has a build volume of 200 mm x 200 mm x 150 mm.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Nicolet Plastics has adopted Mantle’s metal Additive Manufacturing to produce steel production tooling in prototyping time and deliver moulded parts to customers more quickly. The company recently used an AM machine from Mantle to produce production tooling for customer Gamber-Johnson. By additively manufacturing three inserts, Nicolet reduced toolmaker time from 180 hours to 12.5 hours and reduced the time to produce the first moulded parts samples from six to two weeks. Mantle produced inserts that were 95% complete and required only minor finishing before moulding began.

“We printed up the inserts and did a little bit of final fitting here and there, and we were able to get it in the press and start moulding parts relatively quickly,” stated Eric Derner, Nicolet Plastics’ Applications Engineer. “We only had about 10 hours worth of secondary operations and final fitting we had to do. Our tool maker was a little bit pessimistic at first, but when I came in that Friday to ask how everything went, he was almost jumping up and down for joy.”

Additively manufactured H13 inserts from Westec Plastics (Courtesy Mantle)
Additively manufactured H13 inserts from Westec Plastics (Courtesy Mantle)

Westec Plastics Corporation is a full-service plastic injection moulder which has adopted Mantle’s Additive Manufacturing technology to increase its tooling capacity without hiring on toolmakers. Mantle’s technology enables the company to produce H13 tool steel inserts anywhere from 75-95% complete with minimal time from Westec’s toolmakers.

When producing the tooling for a medical diagnostic housing, Mantle’s technology allowed Westec to cut the tooling cost in half by reducing the number of active operation hours on the inserts from 40 hours to 10. The tools were used to mould TPE.

“Tooling is the base of our company,” stated Tammy Barras, president of Westec Plastics. “Without quality tooling, we can’t produce quality parts, but it’s getting harder and harder to find quality tool makers. Using Mantle’s technology, we can complete up to 70% of the job, and have our toolmakers handle the specialised steps that only a human can do. We need to take advantage of this new technology. With Mantle, we can provide our customers a service they can’t get anywhere else.”

www.mantle3d.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
February 20, 2023

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap