HC Starck re-brands its tungsten powders for Additive Manufacturing

MaterialsNews
February 20, 2023
HC Starck has introduced branded tungsten powders for Additive Manufacturing (Courtesy HC Starck Tungsten Powders)
HC Starck has introduced branded tungsten powders for AM (Courtesy HC Starck Tungsten Powders)

HC Starck Tungsten Powders, Goslar, Germany, a subsidiary of Masan High-Tech Materials Group, is now offering its tungsten powders and complementary innovation services for Additive Manufacturing under the brand name starck2print®. The high flowability and optimised particle size distribution are reported to make the powders particularly suitable for AM processes such as Electron or Laser Beam Powder Bed Fusion (PBF-EB and PBF-LB).

The starck2print powders are produced by reducing tungsten oxides in a hydrogen atmosphere. This process contributes to stable production quality at customers’ facilities thanks to the products’ consistently high purity. The company’s extensive recycling expertise also enables the creation of a closed loop within which the tungsten components are recovered from used AM parts and reused as raw materials.

Hady Seyeda, CEO, stated “We believe that metal tungsten has considerable potential in 3D printing. Establishing our own brand underlines our expertise and ambitions in this innovative growth sector.”

www.hcstarck.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
February 20, 2023

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap