Climatic chamber for conditioning metal powders installed at TWI

TWI will use the Weiss Technik climatic chamber to assess the influence of storage conditions, such as the effect of humidity and temperature, on 3D printing metal powders (Courtesy TWI)
TWI will use the Weiss Technik climatic chamber to assess the influence of storage conditions, such as the effect of humidity and temperature, on AM metal powders (Courtesy TWI)

TWI, Cambridge, Cambridgeshire, UK, has acquired a climatic chamber from Weiss Technik, Germany, for the conditioning of metal powders for Additive Manufacturing. The new climatic chamber will be used to assess the influence of storage conditions, such as the effect of humidity and temperature, on AM metal powders as part of IUK funded Scalable AM Rule Creation & Dissemination (SAMRCD) project.

The climatic chamber is capable of simulating various environmental conditions, due to its extended temperature and humidity ranges. Additionally, the climatic chamber allows for rigorous checking and regulation of testing parameters to ensure simulation conditions meet the necessary requirements.

The SAMRCD project operates through a consortium led by Authentise Ltd, London, UK, having been awarded a competitive grant by the UK Research and Innovation’s (UKRI) Transforming Foundation Industries challenge, delivered by Innovate UK. The consortium includes ICD, Materials Processing Institute, TWI and Photocentrics.

TWI will also use the new climatic chamber to help customers simulate a particular environment for metal powders, simulate storage or operating conditions. It will help assess corrosion resistance, evaluate thermal stress and distortions, and understand coating thermal shock response.

www.weiss-technik.com/en

www.twi-global.com

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap