QuesTek awarded $1.2M funding to design niobium-based alloys for AM

QuesTek has been awarded funding to design and develop a novel materials solution for next-generation turbine blade alloys (Courteys QuesTek)

QuesTek Innovations LLC, Evanston, Illinois, USA, has been awarded $1.2 million in funding from the U.S. Department of Energy’s Advanced Research Projects Agency-Energy (ARPA-E). The funding will be used to design and develop a novel materials solution for next-generation turbine blade alloys and compatible coating systems.

The company will design a system of functionally-graded niobium-based alloys suitable for Additive Manufacturing that will be capable of sustaining high-temperature operation, thus increasing fuel efficiency.

Dr Dana Frankel, QuesTek’s Manager of Design and Product Development, commented, “Designing a new turbine material with significantly better performance than current nickel-based superalloys is one of the biggest challenges facing the field of materials science today.”

She added, “We’re excited for this opportunity to apply our proven computational materials design approach to develop a new refractory turbine alloy, paving the way for a step-change in turbine engine performance and efficiency.”

QuesTek explains that it will apply its Integrated Computational Materials Engineering-based models and experience in design of superalloys, refractory alloys, high entropy alloys, and coatings to design a buildable niobium-based multi-material alloy system. Concurrent design of material and component, with the aim of accelerating adoption of the designed materials into next-generation engines, will reportedly be achieved by collaborating with turbine engine manufacturer Pratt & Whitney to define aerospace requirements, perform component design, and guide testing and qualification.

Additionally, the project team includes NASA Jet Propulsion Laboratory for AM process development and the University of Minnesota for coating development.

QuesTek received the award from ARPA-E’s ULtrahigh Temperature Impervious Materials Advancing Turbine Efficiency (ULTIMATE) programme, to develop and demonstrate ultrahigh temperature materials that can operate in the high temperature and high stress environments of a gas-turbine blade.

This effort is said to directly address the need to improve gas turbine efficiency for aerospace and energy applications (e.g., ground-based industrial gas turbines), critical for increasing fuel economy and decreasing carbon emissions. Engine efficiency is fundamentally determined by maximum cycle temperature, and thus scales directly with the operating temperature. However, current state-of-the-art superalloys have limited high-temperature stability, concludes the company.

www.questek.com

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap