Meld Manufacturing Corporation advances in Army Expeditionary Technology Search

Nanci Hardwick, Meld CEO, at the xTechSearch pitch (Courtesy Meld Manufacturing Corporation)

 

Meld Manufacturing Corporation, Christiansburg, Virginia, USA, has been selected for Phase III of the US Army’s Expeditionary Technology Search (xTechSearch), which it initially joined in August 2018. The xTechSearch aims to identify potential collaborators which can work with the army to address the challenges of modernisation; twenty-five technologies across all focus areas were selected by the US Army to advance to Phase III.

Meld’s focus pitch for xTechSearch involved using its patented metal Additive Manufacturing technology to manufacture and repair combat vehicle components and armour. Because Meld machines are operated in an open atmosphere, and reportedly have lower power requirements than competing processes, they can be implemented at both military depots and forward operating bases.

It is expected that the use of Meld could provide the US Army with the strategic ability to make repairs and produce components for combat vehicles as close to the battlefield as possible, while also improving overall efficiency and lowering costs. The Next Generation Combat Vehicle is one of eight US Army technology focus areas for which xTechSearch is seeking novel, disruptive concepts and technologies.

“Meld is a con-ex portable, field-ready technology capable of supporting our warfighters today,” stated Dr Chase Cox, Meld Manufacturing Corporation’s Director of Technology. “Lower-power, safer, easy-to-use equipment capable of repair in the field offers a significant advantage. Before vehicles get to the field, OEM use of Meld can reduce overall price and lead time.”

www.meldmanufacturing.com

News
March 19, 2019

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap