Fraunhofer IGD showcases faster metal AM simulation software at Formnext 2026

Fraunhofer IGD, headquartered in Darmstadt, Germany, will present three software technologies for Additive Manufacturing at Formnext 2026, taking place November 17-20 in Frankfurt.
Among the developments is RISTRA-AM, software used for fast distortion simulation in laser-based metal Additive Manufacturing. According to the company, the GPU-based software delivers simulations 10-100 times faster compared with established CPU-based methods.
This development potentially enables quicker evaluation of build orientations and support structures, helping reduce distortion before manufacturing.

Fraunhofer IGD will also present software developed in collaboration with Fraunhofer ITWM for designing, simulating and optimising parts with tailored properties using unit cells.
The company, alongside the Fraunhofer Institute for Casting, Composite and Processing Technology IGCV, is also set to demonstrate Shape Dithering, a patented geometric method that redistributes voxelisation errors to reduce staircase artefacts. The demonstration uses a binder-jetted sand mould to produce a conventionally cast AlSi7Mg0.3 aluminium component.

“With Shape Dithering, we address the issue not at the hardware level, but in the digital representation of the geometry. Quantisation errors are distributed so that the characteristic staircase artefacts are significantly reduced in the resulting part,” commented Dr Philipp Urban, Head of Research and Development 3D Printing at Fraunhofer IGD.
The three software developments will be exhibited at the joint Fraunhofer Competence Field Additive Manufacturing stand in Hall 11.0, Booth D31.