Converting lunar regolith into materials for Additive Manufacturing

MaterialsNewsResearch
April 28, 2026
Christian Dalsgaard, a Senior Consultant at DTI and the principal investigator of the Regolith to Repairs project (Courtesy Danish Technological Institute)
Christian Dalsgaard, a Senior Consultant at DTI and the principal investigator of the Regolith to Repairs project (Courtesy Danish Technological Institute)

A European Space Agency (ESA) Discovery project, led by the Danish Technological Institute (DTI), is currently investigating how lunar regolith can be converted into materials for Additive Manufacturing of electronic components on the Moon.

The Regolith to Repairs: ISRU for Additive Manufacturing of Electronics project focuses on enabling in-situ production of conductive inks and metal powders from locally available resources. By reducing reliance on Earth-based supply chains, the work aims to support future lunar missions with on-site repair and manufacturing capabilities.

As human missions return to the Moon under programmes such as Artemis, maintaining and repairing critical systems will become essential. Many of these systems depend on electronic circuits, and transporting replacement parts from Earth remains both costly and time-consuming. The DTI-led project addresses this challenge by exploring whether lunar regolith can serve as a feedstock for AM processes.

Lunar regolith contains approximately 40–45% oxygen by weight, chemically bound within its mineral structure. Extracting this oxygen – for use in propulsion or life support – leaves behind a metal-rich residue. The project evaluates whether this residual material can be processed into conductive feedstock suitable for Additive Manufacturing of electronic components.

At the core of the approach is molten salt electrolysis, in which regolith is processed in a calcium chloride electrolyte at temperatures between 800-1,000°C. When a voltage is applied, oxygen is released, leaving metallic alloys. Metalysis, based in Catcliffe, UK, which has collaborated with ESA and the UK Space Agency since 2019, is supplying both untreated and de-oxygenated simulated regolith for the study.

DTI is responsible for converting this metal-rich residue into usable feedstock for Additive Manufacturing. The institute is developing methods to produce conductive inks for AM circuits and metal powders for AM of larger components.

Christian Dalsgaard, Senior Consultant at DTI and principal investigator of the project, explained, “Every time you want to send a kilo into space, you need 15 kg of fuel to move it. There is an enormous advantage in being able to utilise local materials available on the Moon – for example, to repair critical parts.”

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

The ability to manufacture electronics on demand could support a wide range of applications, including maintenance of habitats, repair of robotic systems, and development of communications infrastructure.

“The primary innovation of the project is converting the conductive part of regolith into a digitally printable material,” Dalsgaard added. “This opens new opportunities for off-Earth manufacturing of electronics for future space missions.”

Dr Rita Palumbo, Advanced Manufacturing of Electronics specialist at ESA, stated, “The farther humankind ventures into space, the less we can afford to carry everything we need from Earth. Advanced Manufacturing of Electronics is one of the areas ESA is exploring to understand how future missions might build, repair and adapt electronics.”

To validate the concept, DTI and Metalysis will produce conductive materials from simulated regolith and assess their suitability for Additive Manufacturing. Initial demonstrations will focus on producing conductive features such as wires, with potential applications including antenna fabrication directly on the lunar surface.

While currently a proof-of-concept study, the project forms part of a broader effort to establish regolith as a viable feedstock for electrical components. According to DTI, interest has already been shown by aerospace and defence sector stakeholders.

The project was submitted through ESA’s Open Space Innovation Platform (OSIP) and is funded under the Discovery element of ESA’s Basic Activities programme.

www.esa.int

www.dti.dk

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNewsResearch
April 28, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap