SAE releases ARP7302 standard for closed-loop AM powder sampling

SAE International has released ARP7302 to address powder control in closed-loop metal Additive Manufacturing machines (Courtesy SAE)
SAE International has released ARP7302 to address powder control in closed-loop metal Additive Manufacturing machines (Courtesy SAE)

SAE International, the global standards organisation based in Warrendale, Pennsylvania, USA, has released ARP7302 – Sampling, Conformance Strategies, and Recommended Practices for Closed Loop Processing of Powder for Additive Manufacturing, addressing powder control in closed-loop metal Additive Manufacturing machines.

The Aerospace Recommended Practice (ARP) establishes methods for sampling powder feedstock circulating within closed-loop Additive Manufacturing equipment to demonstrate conformance to a defined powder specification.

The difficulty is that powder within the entirety of closed loop equipment cannot be represented by sampling and testing of discrete, in-process lots. Because powder processing (reconditioning, conveyance, and storage) is asynchronous with a build cycle, individual samples and their associated tests do not represent the totality of powder committed to a machine.

Also, powder consumed as part of an individual build cycle may only represent a subset of feedstock in circulation within such equipment. Therefore, regular testing to substantiate conformance to a powder specification is required to assert conforming feedstock was consumed during individual build cycles of the AM workflow to fabricate parts or preforms.

ARP7302 provides guidance on how to sample and test this circulating powder to support conformance. This is particularly relevant in cases where control frameworks based on key process variables (KPVs) are not implemented or monitored.

The standard outlines recommended approaches including the treatment of powder top-off strategies in closed-loop machines, guidance on sampling both from the machine and from individual build cycles, and terminology intended to support consistency across future SAE standards.

The standard also recognises that, in the absence of defined and controlled KPVs, regular testing is required to substantiate that conforming feedstock has been used during each build cycle. In such cases, evidence of conformance may be required for every build when producing parts.

While other specifications may define control frameworks to maintain powder characteristics – such as atmosphere control and its effect on reactive elements – these approaches are outside the scope of ARP7302.

“ARP7302 is a stepping stone,” explained Tyler LeBrun, PhD, who led the SAE working group responsible for the standard. “AMS7052 is reserved and in drafting as the requirements-laden process specification for continuous closed loop powder reuse, analogous to how AMS7031 governs batch processing of reused powder. A future document covering powder lifing and tracking for closed loop machines, similar in practice to ARP7044, is anticipated but has not yet been reserved as a project.”

The ARP7302 standard is available here.

sae.org

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap