BLT launches high-strength aluminium and titanium alloys for Additive Manufacturing

MaterialsNews
July 18, 2024
BLT recently unveiled two new metal powders tailored for Additive Manufacturing (Courtesy BLT)
BLT recently unveiled two new metal powders tailored for Additive Manufacturing (Courtesy BLT)

Xi’an Bright Laser Technologies Co., Ltd (BLT), Xi’an, China, has introduced a new high-strength aluminium alloy for Laser Beam Powder Bed Fusion (PBF-LB) and a new titanium alloy for PBF-LB and Directed Energy Deposition (DED) Additive Manufacturing.

BLT-AlAM500 aluminium alloy

BLT’s new high-strength aluminium alloy, BLT-AlAM500, is specifically designed for aerospace applications. High-strength aluminium alloys are renowned for their strength, thermal stability, and superior processing performance, making them ideal for aircraft structural components and engine parts. Beyond aerospace, high-strength aluminium alloys are also essential in high-speed trains, lightweight automotive parts, and premium sports equipment.

At TCT Asia 2024, BLT showcased parts made from BLT-AlAM500, these included the bent tube, ventilation duct, and connecting pipe seen below.

The bent tube, ventilation duct, and connecting pipe additively manufactured in BLT-AlAM500 (Courtesy BLT)
The bent tube, ventilation duct, and connecting pipe additively manufactured in BLT-AlAM500 (Courtesy BLT)

These components, characterised by thin-walled, irregularly shaped tubular structures with internal cavities, demand high precision. Traditional manufacturing methods are complex, challenging, and costly. BLT optimised the design for Additive Manufacturing, and used its high-strength aluminium alloy and the company’s BLT-S400 metal PBF-LB machine, to produce the parts. Each component takes approximately thirty hours to form, and achieved an average weight reduction of around 20% compared to the original.

Post-heat treatment, the material achieves tensile strengths of 530-550 MPa, yield strengths of 480-500 MPa, and elongation rates of 11-17%. The material also boasts excellent fracture toughness and fatigue performance, with a room temperature fracture toughness of 30.8 MPa ·m1/2 and a high-cycle fatigue strength of 245 MPa (smooth sample) at room temperature. Compared to similar imported powders, the BLT-AlAM500 material is reported to offer a cost reduction of about 40-50%, significantly lowering manufacturing costs.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

BLT-Ti65 titanium alloy

BLT’s new Ti65 is a multi-component, near-alpha high-temperature titanium alloy, said to maintain excellent strength, plasticity, creep resistance, and thermal stability at temperatures up to 650°C. This performance exceeds the limitations of traditional high-temperature titanium alloys, making Ti65 favoured in aerospace, chemical equipment, and marine engineering applications.

However, Additive Manufacturing Ti65 powder can result in defects such as unmelted or partially melted powder particles, inter-track and inter-layer porosity, and cracking, explains BLT. These can concentrate stress and increase the likelihood of material failure. These difficulties led BLT to develop and introduce its BLT-Ti65 powder.

BLT demonstrated the capabilities of its new BLT-Ti65 titanium alloy by producing a wing cabin sample part, exhibiting high density and no significant defects (Courtesy BLT)
BLT demonstrated the capabilities of its new BLT-Ti65 titanium alloy by producing a wing cabin sample part, exhibiting high density and no significant defects (Courtesy BLT)

The nominal chemical composition of BLT-Ti65 is Ti-5.9Al-4Sn-3.5Zr-0.3Mo-0.4Si-0.3Nb-2.0Ta-1.0W-0.05C, available in 15-53μm (for PBF-LB) and 75-180μm (for DED). Post-heat treatment, parts produced with 15-53μm BLT-Ti65 powder can achieve yield strengths of 483-503 MPa, tensile strengths of 604-624 MPa, and elongation rates of 16.5%-26.5% at 650°C. Parts produced with 75-180μm BLT-Ti65 powder can achieve yield strengths of 478-538 MPa, tensile strengths of 588-648 MPa, and elongation rates of 22%-32% at 650°C.

BLT’s material portfolio now includes over eighty types, including titanium alloys, high-temperature alloys, aluminium alloys, titanium-aluminium alloys, copper alloys, stainless steel, tool steel, high-strength steel, tantalum-tungsten alloys, silver, and hard alloys.

www.xa-blt.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
July 18, 2024

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap