Westinghouse’s Additive Manufacturing improves safety in operating nuclear reactors

ApplicationsNews
July 2, 2024
The fuel assembly bottom nozzle, fabricated using Additive Manufacturing, provides a 30% improvement in debris resistance (Courtesy Westinghouse Electric Company)
The fuel assembly bottom nozzle, fabricated using Additive Manufacturing, provides a 30% improvement in debris resistance (Courtesy Westinghouse Electric Company)

Westinghouse Electric Company LLC, Cranberry Township, Pennsylvania, USA, has used Additive Manufacturing to fabricate bottom nozzles that improve debris capture and fuel endurance within nuclear fuel assemblies. The nozzles, reported to be a nuclear industry first, were integrated into four Lead Test Assemblies delivered to Alabama Power’s Joseph M Farley Nuclear Plant, operated by Southern Nuclear, in the first quarter of 2024.

Debris-wearing action on the fuel rod cladding – known as debris fretting – is the primary source of leaks in pressurised water reactor (PWR) fuel assemblies. Additive Manufacturing technology offers significant improvements in debris filtering thanks to enhanced design freedom which reduces the diameter of debris that can enter into the reactor. In testing, the AM components demonstrated a 30% improvement in debris resistance.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

“Over the past decade, Southern Nuclear has led the industry in the development and implementation of new technologies that improve fuel resiliency,” said Pete Sena, Southern Nuclear President. “The existing nuclear power fleet is the backbone of our country’s clean energy supply, and we are innovating nuclear fuel today to be more robust in order to deliver safer, more affordable and more reliable carbon-free clean nuclear power for decades to come.”

“Our Additive Manufacturing technology is allowing us to achieve breakthrough performance with an immediate positive impact for our customers,” Tarik Choho, Westinghouse President of Nuclear Fuel, shared. “This significant technology innovation for PWR reactors mitigates the risk of leakage in the fuel rods due to the accumulation of debris, strengthening the safety and efficiency of our customers’ operations.”

In 2015, Westinghouse conducted one of the first material irradiation studies of additively manufactured nuclear components. In 2020, Westinghouse installed its first-ever safety-related AM component, a Thimble Plugging Device, into an operating commercial reactor, and in 2024 Westinghouse produced the 1,000th additively manufactured flow plate for VVER-440 fuel assemblies.

www.westinghousenuclear.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
July 2, 2024

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap