SSAB launches Armox 500 AM steel powder for armour applications

MaterialsNews
June 17, 2026
Camera turret additively manufactured with Armox 500 AM powder, ready for use as built (Courtesy SSAB)
Camera turret additively manufactured with Armox 500 AM powder, ready for use as built (Courtesy SSAB)

Swedish steel company SSAB has launched Armox 500 AM, a high-strength steel powder optimised for Additive Manufacturing. The material is particularly suited to protective armour applications where conventional armour plate solutions may not be suitable.

Armox protection plate has been used in armour applications for more than four decades, and SSAB states that Armox 500 AM is the first steel powder to match its properties. The company reports that the material has already attracted interest from customers in the defence sector.

“The demand for protection steel is growing globally, and SSAB’s unique offerings give us a leadership position with customers in the defence industry. In addition, demand for high-performance metal powders for Additive Manufacturing is growing,” stated Per Elfgren, Head of SSAB Special Steels. “We have developed our own high-strength steel powders optimised for Additive Manufacturing, based on many decades of experience in high-performance steel products. This enables advanced designs with low weight and high strength.”

Design freedom beyond the armour plate

According to SSAB, components produced using Armox 500 AM powder can provide ballistic and blast protection while enabling geometries that are difficult or impossible to manufacture using conventional machining and fabrication methods.

Potential applications include solid components, such as hinges and housings, as well as structures incorporating internal lattice or honeycomb geoqmetries. Such designs can be developed using Design for Additive Manufacturing (DfAM) principles to reduce weight, while maintaining structural performance and protective capability.

SSAB suggests that Additive Manufacturing can be used to create customised protective structures for vulnerable external systems on military vehicles and equipment. These may include cameras, antenna mounts, optical sights, radar systems, hydraulic couplings and cable connections.

The company states that components produced using Armox 500 AM powder can achieve the required mechanical and protective properties without the need for subsequent heat treatment.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

Production expansion planned

Armox 500 AM powder is produced at SSAB’s steelworks in Oxelösund, Sweden, where the company also manufactures additional steel powder grades. According to SSAB, Armox 500 has undergone testing for flowability, particle morphology and particle size distribution. The company has also produced and evaluated a range of demonstration components to assess ballistic and blast resistance.

SSAB plans to expand its powder production facility in Oxelösund during 2026 to support commercial-scale manufacturing. Production capacity is expected to increase progressively from the first quarter of 2028, with a planned annual output of approximately 350 tonnes.

www.ssab.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
June 17, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap