NSL reports complete material analysis with ICP and LECO

Inductively Coupled Plasma (ICP) testing is a leading industry method for testing the elemental composition of materials. ICP utilises one or both of two techniques (ICP Mass Spectrometry or ICP Optical Emission Spectrometry) to precisely detect and measure elements in a wide range of materials from advanced metal alloys and ceramics on aeroplanes, to pharmaceuticals and cosmetics (Courtesy NSL Analytical Services)
Inductively Coupled Plasma (ICP) testing is a leading industry method for testing the elemental composition of materials. ICP utilises one or both of two techniques (ICP Mass Spectrometry or ICP Optical Emission Spectrometry) to precisely detect and measure elements in a wide range of materials from advanced metal alloys and ceramics on aeroplanes, to pharmaceuticals and cosmetics (Courtesy NSL Analytical Services)

NSL Analytical Services, Inc., based in Cleveland, Ohio, has shared a case study by Dr Ross Cunningham, Director of Science and Technology at NSL Analytical Services, Inc., exploring how Inductively Coupled Plasma (ICP) analysis and LECO (which includes Combustion Analysis and Inert Gas Fusion) testing deliver complete material analysis. ICP and LECO testing are two industry-leading methods for testing elemental composition of a wide variety of materials, ranging from enhanced metal alloys and ceramics on aircraft to pharmaceuticals and cosmetics.

Each method brings a unique capability to accurately generate compositional information on most material systems. ICP is capable of detecting bulk and trace elements across the majority of the periodic table, while LECO is used to detect light elements, like oxygen and nitrogen, that ICP is unable to measure. When used together, they provide nearly the whole spectrum of elements from bulk to trace levels, ensuring a high confidence of material quality and regulatory compliance.

These techniques are believed to be essential tools for engineers and manufacturers, offering fast, accurate and repeatable results, and require only a small amount of test material. As a result, they enable enhanced quality control and assurance at every stage of the production cycle, from raw materials to end products.

What are the methods and principles behind ICP testing?

Depending on the required detection range (the percentage of an element of interest, from bulk to ultra-trace), ICP testing utilises one or both of two techniques to precisely detect and measure elements in a wide range of materials. If the sample is initially solid, it is first dissolved in an acid to form a liquid solution. Each technique involves vaporising, atomising and ionising the liquid sample by injecting it into an argon plasma formed by a radio frequency generator, known as an Inductively Coupled Plasma, or ‘ICP’.

Optical Emission Spectroscopy (ICP-OES), otherwise known as Atomic Emission Spectroscopy (ICP-AES), operates on the principle that excited atoms emit light at specific characteristic wavelengths. In this technique, the liquid sample is injected as an aerosol into the plasma, where the intense heat vaporises the sample and ionises the atoms therein. When the ions return to their ground state, they release the energy as photons of light, whose intensity is measured with photomultiplier tubes (PMTs) or charge-coupled devices (CCDs). The wavelength of an emitted photon is characteristic of the specific element, while the intensity is proportional to its concentration. This allows for accurate, quantitative analysis of a wide spectrum of elements simultaneously.

Mass Spectrometry (ICP-MS) combines the high-temperature ionisation capabilities of ICP with mass spectrometer detection. It is similar to ICP-OES in that the sample is introduced into an argon plasma to be atomised and ionised but is unique in that this method directly measures the ions the plasma produces.

The charged ions are then extracted through an interface (typically a pair of water-cooled cones) and directed through ion optics (electrostatic lenses) that guide the ions into a mass analyser where the ions are separated and measured based on their mass-to-charge ratio, or m/z value. The signal generated is directly proportional to the relative concentration of the element in the sample, which is converted to a concentration by comparing it to a calibration standard of a known value.

LECO testing is the common brand name for equipment that utilises Combustion Analysis or Inert Gas Fusion to identify specific light elements that are generally not measurable by ICP (Courtesy NSL Analytical Services)
LECO testing is the common brand name for equipment that utilises Combustion Analysis or Inert Gas Fusion to identify specific light elements that are generally not measurable by ICP (Courtesy NSL Analytical Services)

How does LECO testing work in elemental analysis?

While powerful in its breadth of elements and range of detection limits, ICP is not capable of detecting all elements. This is where LECO testing comes in, which is the common brand name of equipment for methods that utilise Combustion Analysis or Inert Gas Fusion to identify specific light elements in a sample that are generally not measurable with ICP, namely for C, S, O, N and H.

Combustion analysis heats a small sample to a high temperature in an oxygen-rich environment, converting Carbon and Sulfur into their gaseous oxides, like CO2, which are measured using an infrared absorption detector (NDIR).

Inert gas fusion heats the sample in an inert atmosphere, such as helium or argon, to release nitrogen, oxygen, and hydrogen. These elements are then processed through a series of catalysts, detectors, and scrubbers to independently analyse the constituent elements.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

Why are ICP and LECO testing valuable to manufacturers?

These testing methods ensure that the raw materials and finished products meet precise specs for elemental composition. This is a key consideration for performance-critical industries like aerospace and defence, automotive, and medical devices, because users are now demanding more from materials, and even the smallest out-of-spec variations in trace elements like carbon or sulfur content can impact the material’s properties and fitness-for-use, ultimately undermining the safety or performance of the product.

Accurate and repeatable elemental analysis allows manufacturers to meet strict compliance and specification targets through each stage of the product lifecycle, whether it’s R&D, quality assurance or failure analysis. While invaluable in making sure elements are present in the appropriate concentrations in alloys and materials, they are equally useful in ensuring contaminants like oxygen or sulfur in alloys or dangerous elements, like lead or mercury, are absent or below acceptable limits for medical or consumer-facing products.

www.nslanalytical.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap