Lufthansa Technik and Materialise develop Ti6Al4V AM latch for Airbus aircraft

The Ti6Al4V latch developed by Lufthansa Technik and manufactured by Materialise for Airbus A330, A340 and A380 roller shutter assemblies (Courtesy Materialise)
The Ti6Al4V latch developed by Lufthansa Technik and manufactured by Materialise for Airbus A330, A340 and A380 roller shutter assemblies (Courtesy Materialise)

Lufthansa Technik, Hamburg, Germany, has worked with Materialise, headquartered in Leuven, Belgium, to produce a Ti6Al4V replacement for a polymer latch used in roller shutter assemblies on Airbus A330, A340 and A380 aircraft.

The project followed repeated in-service damage to the roller shutter assemblies, which was traced to the original polymer latch. The latch retains the roller brake and endcap within the roller shutter assembly, but according to the case study, it could not be purchased individually from the original equipment manufacturer. As a result, failure of the component could require replacement of the complete roller shutter assembly.

Lufthansa Technik therefore redesigned the latch for metal Additive Manufacturing to produce a replacement component separately from the complete assembly.

“The original part was an injection molded polymer component with a complex geometry,” stated David Rudolz, Project Engineer at Lufthansa Technik. “It was immediately identified as an ideal candidate for metal Additive Manufacturing.”

The original polymer latch was redesigned in Ti6Al4V (Courtesy Materialise)
The original polymer latch was redesigned in Ti6Al4V (Courtesy Materialise)

The redesign had to reproduce the function of the original polymer component while accounting for the different mechanical behaviour of Ti6Al4V. Lufthansa Technik stated that the elastic response of the titanium alloy, geometry and wall thickness of the redesigned latch were considered during development.

Following the selection of Ti6Al4V for the application, Lufthansa Technik chose Materialise to manufacture the component. Materialise subsequently underwent a supplier audit and was qualified by Lufthansa Technik for the production of metal Additive Manufacturing parts.

The two companies worked together on manufacturing requirements, process stability and production controls. Materialise states that the parts were manufactured in accordance with its EN 9100 certification and Lufthansa Technik’s design requirements, and are now certified for flight use and in service.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

According to the companies, replacing the polymer component with the Ti6Al4V design is expected to increase the latch’s service life. The availability of the component as an individual replacement part also enables Lufthansa Technik to repair the roller shutter assembly rather than replace the complete unit.

Following the project, Materialise has also been named an official ‘workbench’ for metal parts by Lufthansa Technik.

www.materialise.com

www.lufthansa-technik.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap