Innospace validates bi-propellant cooling technology

ApplicationsNews
August 5, 2026
The combustion chamber of the methane engine combustor manufactured at Innospace’s in-house metal Additive Manufacturing facility at its Hwaseong Campus (Courtesy Innospace)
The combustion chamber of the methane engine combustor manufactured at Innospace’s in-house metal Additive Manufacturing facility at its Hwaseong Campus (Courtesy Innospace)

Innospace, headquartered in Sejong, South Korea, has successfully completed a 420-second ground firing test featuring its bi-propellant regenerative cooling methane rocket engine technology. The test, reportedly the longest-duration test of its kind conducted in South Korea, was undertaken to verify the durability and robustness of a methane engine incorporating the new additively manufactured technology.

Developed for the company’s 0.4-tonne-thrust (approximately 3.9 kN) liquid methane engine, LiMEK-04, it is intended for use in the kick stage of Innospace’s next-generation HANBIT-Micro launch vehicle. The kick stage is designed to separate following second-stage engine shutdown and deliver payloads to their designated orbits with greater precision.

The newly developed system employs a bi-propellant regenerative cooling architecture that uses both liquid methane fuel and liquid oxygen (LOx) as coolants for the combustion chamber. Regenerative cooling is a critical rocket propulsion technology that protects engine components from the extreme temperatures generated during combustion while supporting stable operation and performance.

Conventional methane rocket engines typically use liquid methane alone as a coolant. According to Innospace, this approach often requires higher propellant feed pressures to achieve adequate cooling performance, resulting in heavier tanks and feed systems.

Nuclear Fusion’s Manufacturing Challenge Where Metal Additive Manufacturing Can Make The Difference

By utilising both liquid methane and liquid oxygen during the cooling process, the company’s technology reportedly increases coolant flow rates by approximately 3-3.4x compared to conventional single-propellant systems. Innospace states that this enables effective cooling at lower operating pressures, potentially reducing the mass of tanks and feed systems and improving overall launch vehicle efficiency.

“As launch vehicles become smaller, mass efficiency becomes increasingly critical,” stated Soojong Kim, founder and CEO of Innospace. “With global demand for small-space propulsion systems continuing to grow, we expect this technology to have broad applicability not only in methane engines for reusable launch vehicles, but also in kick stages for small satellite orbital transfer missions and future space exploration propulsion systems.”

www.innospc.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
August 5, 2026

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap