Farsoon Technologies announces new metal Additive Manufacturing machine
Farsoon Technologies has announced its new FS271M metal Additive Manufacturing machine aimed at demanding applications in the aerospace, automotive and medical sectors. Incorporating a 500W Yb-fibre laser, the new system offers high-accuracy custom scanning algorithms and a 275 x 275 x 320 mm build area.
The FS271M offers complete access to machine parameters and settings, offering customers the choice of utilising Farsoon materials or the wide range of third-party materials available. In addition to fabricating nearly any metal powder, the FS271M incorporates the latest safety systems with inert gas supply and over-sized protective filter systems.
Hunan Farsoon High-tech Co., Ltd, headquartered in China, was founded in 2009 and specialises in the development and manufacture of Selective Laser Sintering (SLS) equipment and materials. The company’s open platform strategy allows for complete freedom to operate with any open platform application or development programme.