Cold spray as a Powder Metallurgy process for the production of nickel aluminium bronze

Microstructure of as-sprayed alloy (a) binary aluminium bronze (b) nickel aluminium bronze (Courtesy Camilleri S, Tran T, Duguid A, Krishnan K (2025) Cold spray as a Powder Metallurgy process for production of nickel aluminium bronze.
Microstructure of as-sprayed alloy (a) binary aluminium bronze (b) nickel aluminium bronze (Courtesy Camilleri S, Tran T, Duguid A, Krishnan K (2025) Cold spray as a Powder Metallurgy process for production of nickel aluminium bronze.

Australian researchers from SPEE3D, headquartered in Melbourne, and Charles Darwin University, Darwin, Australia, have published a paper in PLOS One focused on the use of Cold Spray Additive Manufacturing in the production of nickel aluminium bronze (NAB) alloys over the traditional Powder Metallurgy technique.

In the study, both binary aluminium bronze (AB) and NAB alloys were produced using powders, additively manufacturing components via cold spray and then heat treating the resultant parts. The AB alloy contained blended 9.9% aluminium alloy (Al6061) powder and copper powder, while the NAB alloy included 11% Al6061 powder, 5.8% nickel powder, 6.8% iron powder, and copper powder.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Powders were mixed under controlled conditions and deposited using a LightSPEE3D AM machine and compressed air. Post-deposition heat treatments – such as homogenisation, ageing, and/or Hot Isostatic Pressing (HIP) – were applied to enhance material properties.

According to the researchers, their results showed that Cold Spray Additive Manufacturing combined with suitable heat treatments can produce NAB alloys with desirable microstructures containing fine κ phases and mechanical properties with above 280 MPa yield strength, above 500 MPa tensile strength and 20% elongation. This dataset is comparable to numbers achieved by traditional cast methods – which results in yield strength of 240 MPa, tensile strength of 580 MPa and 15% elongation – and better results than those produced via PM.

The study also noted that replacing solution treatment at HIP process at 1035°C can further enhance the mechanical properties of NAB samples produced via Cold Spray Additive Manufacturing, making them superior to traditionally cast NAB materials. This highlights the potential of cold spray AM to produce high-performance materials more efficiently.

‘Cold spray as a Powder Metallurgy process for the production of nickel aluminium bronze’ is available here, in full.

www.spee3d.com

www.cdu.edu.au

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap