RMIT researchers use titanium Additive Manufacturing to create exceptionally high-strength metamaterial
Researchers from RMIT University in Australia have reported the development of a new type of metamaterial, additively manufactured from Ti-6Al-4V titanium alloy. Boasting exceptionally high levels of strength ... Read more »