Freemelt, Sandvik and Mid Sweden University join to accelerate PBF-EB Additive Manufacturing
A strategic collaboration, between Sweden’s Freemelt AB, Sandvik AB and Mid Sweden University, is aiming to establish Electron Beam Powder Bed Fusion (PBF-EB) Additive Manufacturing as an innovative and competitive ... Read more »