ProFocus six-laser DED titanium components with m4p’s Ti-6Al-4V powder
Oscar-PLT GmbH, Klipphausen, Germany, and m4p material solutions GmbH, Magdeburg, have published the results of a joint project on the production of Ti-6Al-4V via Oscar’s ProFocus Directed Energy Deposition ... Read more »