Xact Metal expands into Brazil through 3DCRIAR sales partnership
Xact Metal, headquartered in State College, Pennsylvania, USA, has announced a sales and service partnership with Additive Manufacturing solutions provider 3DCRIAR, based in Sāo Paolo, Brazil. ... Read more »