Arcam EBM to expand into new facility
Arcam AB, a GE Additive company, has signed a lease agreement with Castellum for its Additive Manufacturing machine business to move into a refurbished 11,800 m2 facility in Härryda, outside Göteborg, Sweden.
This new facility is said to be almost three times the size of the current site, and is expected to offer Arcam EBM the ability to continue to expand and set the stage for the accelerated growth of the Additive Manufacturing industry.
The space will significantly increase machine production capacity and allow for a more collaborative set-up within the company; uniting logistics, research and development, services and operations. The facility will be ready for move-in the first quarter for 2019.
The expansion for Arcam EBM follows on that Arcam in September 2017 inaugurated a new powder manufacturing plant at AP&C in Canada.