Westinghouse celebrates 1,000th additively manufactured fuel flow plate for nuclear reactors

Westinghouse Electric Company has manufactured its 1,000th fuel flow plate using Additive Manufacturing (Courtesy Westinghouse Electric Company)
Westinghouse Electric Company has manufactured its 1,000th fuel flow plate using Additive Manufacturing (Courtesy Westinghouse Electric Company)

Westinghouse Electric Company LLC, a nuclear energy technology provider headquartered in Cranberry Township, Pennsylvania, USA, recently manufactured its 1,000th fuel flow plate using Additive Manufacturing. The fuel flow plate is reported to the first-ever safety-related AM component to enter serial production for the nuclear industry.

The additively manufactured flow plates are installed in VVER-440 fuel assemblies, enabling a redesign of the assemblies’ bottom part which is said to result in a more robust performance.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

“This achievement showcases the development of Additive Manufacturing from prototyping to full-scale production, generating tangible value for our customers,” stated Lou Martínez Sancho, Westinghouse Chief Technology Officer and Executive Vice President, R&D and Innovation. “This marks another Westinghouse pioneering achievement in AM Technology holding the commitment to strengthen safety, efficiency, sustainability and energy security.”

In 2015, Westinghouse conducted a material irradiation study of AM nuclear components and in 2020, the company installed a safety-related additively manufactured component — a thimble plugging device — into an operating commercial reactor.

Westinghouse supplied the world’s first commercial pressurised water reactor in 1957 and the company’s technology is the basis for nearly half of the world’s operating nuclear plants.

www.westinghousenuclear.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap