NASA’s GRX-810 alloy undergoes successful hot-fire testing for liquid rocket engines

Fig. 1 Hot-fire testing of GRX-810 injectors and nozzles for the ORCA liquid oxygen/liquid methane test series (Courtesy NASA/AIAA SciTech 2024)
Fig. 1 Hot-fire testing of GRX-810 injectors and nozzles for the ORCA liquid oxygen/liquid methane test series (Courtesy NASA/AIAA SciTech 2024)

NASA first reported the development of its GRX-810 powder in 2022, an oxide dispersion strengthened (ODS) alloy specifically for use in extreme temperatures. This Ni-Co-Cr based alloy was designed for aerospace applications, including liquid rocket engine injectors, preburners, turbines, and hot-section components, where it is required to withstand temperatures up to 1100°C.

The alloy was created using integrated computational materials engineering techniques to focus on a new class of materials that provide exceptional temperature and oxidation-resistant properties. GRX-810’s aim is to bridge the temperature gap between traditional nickel-base superalloys and refractory alloys.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

The GRX-810 alloy utilises Additive Manufacturing to incorporate nano-scale yttria particles throughout its microstructure and, compared to traditional nickel-base superalloys, is said to provide a two-fold increase in tensile strength, 1,000-fold better creep properties, and two-fold improvement in oxidation resistance.

As discussed in a paper presented at the 2024 AIAA Science and Technology Forum and Exposition (AIAA SciTech Forum), January 8-12, 2024, Orlando, Florida, USA, a team of NASA researchers led by Paul R. Gradl, Combustion Devices Manufacturing and Design Engineer at NASA’s Marshall Space Flight Center in Huntsville, USA, confirmed a successful series of hot-fire tests using liquid oxygen/liquid hydrogen (LOX/LH2) and liquid oxygen/liquid methane (LOX/LCH4) propellants. Rigorous high-duty cycle testing of various injectors and nozzles was reported to have demonstrated improved life compared to traditional nickel-base superalloys.

The authors explained that a coating process for the powder feedstock was refined to enhance the high-temperature properties of GRX-810. This involved coating pre-alloyed base powder with <1 wt.% Y2O3 nanoparticles, ensuring even dispersion when additively manufactured using Laser Beam Powder Bed Fusion (PBF-LB).

The ODS coating, achieved through AM, was said to address the historical cost challenges associated with traditional ODS alloy production and resulted in a well-distributed and stabilised microstructure at elevated temperatures. It was stated that a single heat treatment using Hot Isostatic Pressing (HIP) minimises grain growth, further enhancing the material’s structural integrity.

Fig. 2 Various components built using GRX-810 PBF-LB: A) turbine blisk, B) inducer with internal features, C) impinging injector, D) regeneratively-cooled nozzle, E) shrouded turbine blisk, F) larger-scale turbine blade with integral instrumentation ports (Courtesy NASA/AIAA SciTech 2024)
Fig. 2 Various components built using GRX-810 PBF-LB: A) turbine blisk, B) inducer with internal features, C) impinging injector, D) regeneratively-cooled nozzle, E) shrouded turbine blisk, F) larger-scale turbine blade with integral instrumentation ports (Courtesy NASA/AIAA SciTech 2024)

The GRX-810 components used in the hot-fire test were additively manufactured on an EOS M280 using atomised feedstock from Praxair. Testing was conducted at NASA MSFC test stand 115 under the Optimised and Repeatable Components using Additive (ORCA) development project and Reactive Additive Manufacturing for the Fourth Industrial Revolution (RAMFIRE) collaboration. The RAMFIRE test series incorporated the GRX-810 injector shown in Fig. 2, whereas the ORCA test series used both a GRX-810 injector and nozzle (Fig. 3).

Fig. 3 Thrust chamber assembly configuration for the ORCA test series (Courtesy NASA/AIAA SciTech 2024)
Fig. 3 Thrust chamber assembly configuration for the ORCA test series (Courtesy NASA/AIAA SciTech 2024)

Liquid oxygen/liquid hydrogen and liquid oxygen/liquid methane versions of GRX-810 pentad injectors using a centre-mounted torch igniter were built. Two truncated ideal contour GRX-810 nozzles were fabricated as well. The injectors accumulated 3,117 seconds of hot fire across pressures of 37.4 to 57.2 bar, and the nozzles accumulated over 2,458 combined seconds.

The authors concluded that the successful application of GRX-810 alloy in hot-fire testing, particularly in LOX/LH2 and LOX/LCH4 environments, demonstrated its robustness and readiness for aerospace applications.

Future work involves additional scaling and analysis of the GRX-810 alloy feedstock and both PBF-LB and laser powder-based DED builds for large-scale production and broader applications. NASA plans to continue the maturation of the GRX-810 alloy into component applications, with the final goal of commercialisation. Research efforts are said to be exploring additional applications within aerospace and the energy industry.

The full paper, “Extreme Temperature Additively Manufactured GRX-810 Alloy Development and Hot-fire Testing for Liquid Rocket Engines,” published by the American Institute of Aeronautics and Astronautics, can be downloaded here.

www.nasa.gov

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap