Personalised titanium smart watch housings developed by Incus and Element22

ApplicationsNews
January 5, 2024
Sintered titanium smart watch housing before surface modification (Courtesy Incus/Element22)
Sintered titanium smart watch housing before surface modification (Courtesy Incus/Element22)

Gerald Mitteramskogler, CEO of Incus GmbH, Vienna, Austria, has highlighted the potential of lithography-based metal manufacturing (LMM) technology, defined as a vat photopolymerisation process (VPP) by ISO/ASTM, in a detailed look at the production of personalised titanium smart watch housings. Working with Element22 GmbH, based in Kiel, Germany, the partners recognised the challenges of processing Ti64 in binder- or sinter-based Additive Manufacturing processes.

The R&D project resulted in a feedstock consisting of Ti64 powder at 55Vol% solids loading. The binder undergoes photopolymerisation during light irradiation, which results in the formation of a green part layer-by-layer. The green strength of the parts produced using LMM technology is said to be typically around 13 MPa in a three-point-bending setup, which is higher than other sinter-based AM processes. This high green strength allows for automated handling during extraction or de-powdering, and also facilitates the placement of the green parts onto the sintering setter, explained Mitteramskogler.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

During the debinding and sintering process, the binder is thermally decomposed, leaving only the metal powder behind. A solids loading of 50Vol%+ is typically required to achieve dense and mechanically functional parts, which can be sintered to produce final solid materials with theoretical densities exceeding 99%. The LMM process results in a surface finish as low as 2µm Ra (as-sintered) and a resolution of 35 µm.

The watch housings undergoe a sandblasting stage before being coloured (Courtesy Incus/Element22)
The watch housings undergoe a sandblasting stage before being coloured (Courtesy Incus/Element22)

In addition to developing a low-carbon photopolymer-based binder system, an adapted thermal processing route for Ti64 was also achieved. The resulting Ti64 is said to showcase ‘remarkable’ mechanical properties, exceeding ASTM F2885-17 standards for medical implant applications.

Beyond the advantages of mass customisation, LMM is said to result in MIM-like quality parts within hours, rather than weeks. Matthias Scharvogel, CEO of Element22, added, “Being a user of LMM, we can achieve significant savings in time to market for our customers, especially for high-quality prototypes and mass customisation.”

Incus’ HammerPro40 AM machine can reportedly build up to sixteen watch cases in less than 2.5 hours, with an annual production capacity of approximately 35,000 pieces. Once sintered, the watch housing undergoes a sandblasting stage before being coloured.

“With a fully customised smartwatch housing, we can achieve a competitive cost structure compared to traditional manufacturing technologies, especially when designs can no longer be realised with MIM or CNC,” Mitteramskogler concluded.

The full report is available here.

www.incus3d.com

www.element22.de

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
January 5, 2024

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap