IperionX receives $12.7 million DoD grant to boost titanium powder production for US defense supply chains

MaterialsNews
November 1, 2023

The United States Department of Defense (DoD) has announced it is awarding $12.7 million to IperionX Technology, LLC. Facilitated through the Defense Production Act Investment (DPAI) Program, the award aims to increase titanium powder production for defence supply chains.

“Robust and resilient defense supply chains are critical to the Warfighting capability of the United States,” stated Dr Laura Taylor-Kale, Assistant Secretary of Defense for Industrial Base Policy. “Domestic titanium production is a top priority for the DoD’s industrial base programs.”

The award will fund the expansion of IperionX’s facility in Virginia into a demonstration plant, boosting the company’s titanium powder production to 125 metric tons annually. Within five years, IperionX aims to produce 10,000 metric tons of titanium metal powder each year. The company manufactures titanium alloys from either titanium minerals or 100% recycled materials.

As of 2023, the DPAI Program has granted twenty-one awards totalling $674 million. DPAI is overseen by the ASD(IBP)’s Manufacturing Capability Expansion and Investment Program (MCEIP), in the Office of the Deputy Assistant Secretary of Defense for Industrial Base Resilience.

www.defense.gov

iperionx.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
MaterialsNews
November 1, 2023

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap