Royal Air Force exploring Additive Manufacturing for aerospace parts

ApplicationsNews
July 21, 2023
Examples of additively manufactured components selected by the RAF (Courtesy AS1 Kimberley Waterson/RAF)
Examples of additively manufactured components selected by the RAF (Courtesy AS1 Kimberley Waterson/RAF)

As reported in Aviation Week, the UK Royal Air Force is said to be experimenting with Additive Manufacturing in hopes to provide a way to produce urgently needed aerospace parts. Project Warhol, a team of four focused on Additive Manufacturing, has been funded by the Rapid Capabilities Office and the UK Defence Innovation Fund.

It is hoped that Additive Manufacturing could help reduce the reliance on contested logistics systems and make platforms more readily available when deployed overseas. Establishing Additive Manufacturing capabilities on the Royal Air Force’s bases would build on the capacity provided by station workshops performing precision metalwork.

Reportedly, the team hoped to have already flown its first in-house-produced part, a blanking plate, on an in-service Airbus Puma helicopter prior to the Royal International Air Tattoo. However, the component is undergoing a clearance process with military airworthiness authorities and is expected to fly shortly.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Chief Technician Mike Matthias, told Aviation Week, “This is not about producing main spars for combat aircraft, but creating components we can then ship to support forward assets.”

The team is believed to be developing its capability by using an Electron Beam Powder Bed Fusion (PBF-EB) machine for titanium, and a Laser Beam Powder Bed Fusion (PBF-LB) machine for aluminium parts. However, it is aware of the challenges in certification and intellectual property when producing alternative parts to those provided by OEMs. One possibility is to purchase the digital design files from the manufacturer for future iterations of the team, allowing production of the part as needed.

Project Warhol has reportedly been tasked with assessing the technology until March 2024, with the potential to extend the project. A final assessment is due by March 2025, at which point a decision will be made regarding AM’s capability within the RAF’s core budget.

www.raf.mod.uk

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
July 21, 2023

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap