Rosswag now TÜV SÜD certified for Additive Manufacturing of pressure equipment

News
April 21, 2023
The team at Rosswag Engineering with the TÜV SÜD certification for the Additive Manufacturing of components made of 316L stainless steel (Courtesy Rosswag Engineering)
The team at Rosswag Engineering with the TÜV SÜD certification for the Additive Manufacturing of components made of 316L stainless steel (Courtesy Rosswag Engineering)

Rosswag Engineering, Pfinztal, Germany, has been certified by TÜV SÜD for the Additive Manufacturing of components made of 316L stainless steel (1.4404) according to the European PED (Pressure Equipment Directive) 2014/68/EU.

Rosswag Engineering is one of the first manufacturers in the world to gain this certification, and to achieve this, the company completed the extensive testing and certification programme in accordance with DIN 17026:2020. Essentially, the quality of the entire process is certified – from the consistency of the manufacturing processes to the internal processes for quality assurance and quality controls to the reproducibility of the mechanical-technological properties, considering the PED requirements.

In order to meet the high quality demands of additively manufactured pressure equipment, more than 100 specimens were produced on the SLM® 280 2.0 Laser Beam Powder Bed Fusion (PBF-LB) Additive Manufacturing machine and subsequently tested.

“We want to offer solutions to transfer more functional optimised and additive manufactured components into industrial applications,” stated Gregor Graf, Head of Engineering at Rosswag GmbH. “But to be able to apply innovative heat exchangers, for example, there was no alternative to certification according to the Pressure Equipment Directive.”

Gunther Kuhn, Head of Product Management at TÜV SÜD Industry Service GmbH, added, “With our certification according to the Pressure Equipment Directive, we can also confirm the high quality, reliability and safety of Rosswag GmbH’s additive manufactured products for the end user.”

www.rosswag-engineering.de

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
News
April 21, 2023

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap