Czinger Vehicles and Xtrac develop additively manufactured gearbox for 21C hypercar

ApplicationsNews
March 16, 2023
The additively manufactured gearbox is currently undergoing validation in the Czinger 21C and Vmax hypercars (Courtesy Czinger Vehicles)
The additively manufactured gearbox is currently undergoing validation in the Czinger 21C and Vmax hypercars (Courtesy Czinger Vehicles)

Czinger Vehicles has partnered with motorsport gearbox specialist Xtrac to produce an additively manufactured high-performance gearbox case for use in its 21C hypercar. The topology-optimised gearbox is manufactured from a proprietary aluminium alloy, reportedly leading to significant weight savings, outstanding structural performance & production quality, and efficient manufacturing times.

The gearbox is built using the Divergent Adaptive Production System (DAPS), a software/hardware solution from Divergent, which is designed to replace traditional vehicle manufacturing. The DAPS approach eliminates the need for tooling, enabling a reduction in development time and the ability to make real-time design improvements.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

Based in Berkshire, UK, and with US facilities in Indiana and North Carolina, Xtrac develops and manufactures world-leading transmission and driveline products, including gearboxes, differentials, and gearchange systems. Since 1984, over 1,200 gearbox designs have been produced, with many used in top-level professional motorsport globally. Partnering with Xtrac to engineer and develop the 21C’s additively manufactured gearbox is anticipated to further boost the 21C’s performance.

The Czinger 21C incorporates over 350 metal additively manufactured components and structures throughout the car, from the vehicle’s chassis to brake, suspension and exhaust components (Courtesy Czinger Vehicles)
The Czinger 21C incorporates over 350 metal additively manufactured components and structures throughout the car, from the vehicle’s chassis to brake, suspension and exhaust components (Courtesy Czinger Vehicles)

“We are proud to team Czinger’s world-class engineers with those at Xtrac,“ stated Lukas Czinger, Czinger Co-Founder and SVP Operations. “Together, we have developed an incredible, industry-first gearbox that is truly at the pinnacle of performance. We can’t wait to shatter more track records as we utilise this system in the 21C.”

The topology-optimised gearbox is manufactured from a proprietary aluminum alloy and will be used in the 21C hypercar (Courtesy Czinger)
The topology-optimised gearbox is manufactured from a proprietary aluminum alloy and will be used in the 21C hypercar (Courtesy Czinger)

The gearbox features the following performance specifications:

  • Automated 7‑speed, semi‑sequential gearbox
  • First 48V‑electrically actuated twin barrel system, resulting in what is reputed to be the fastest automated single-clutch synchromesh gearbox
  • Dual barrel gear actuation allows for smoother EV‑to‑rear drive blending for easier city driving
  • Sub‑100 ms shifts combined with blending of front‑axle EV power allow for easy shifts for high-performance driving.
  • Reputedly features the highest torque transmitted per mass of gearcase for any road‑legal vehicle

“What our Xtrac engineers have accomplished in tandem with Czinger and Divergent is groundbreaking. Xtrac is pleased to be at the forefront of cutting-edge gearbox manufacturing by creating these 3D printed casings. It has been extremely interesting and very stimulating for our engineers working closely together to bring this cutting edge innovation to life,” Adrian Moore, CEO, Xtrac.

www.xtrac.com

www.czinger.com

Discover more about how Czinger Vehicles is using Divergent’s technology in our article ‘How the Czinger 21C is redefining next-generation car manufacturing’, first published in Metal AM Vol 7 No 4, Winter 2021

ApplicationsNews
March 16, 2023

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap