AIM Sweden shortens valve manufacturer’s lead times with Additive Manufacturing

ApplicationsNews
February 16, 2023
Ramén is using Additive Manufacturing to build a range of industrial control valves (Courtesy Ramén Valves)
Ramén is using Additive Manufacturing to build a range of industrial control valves (Courtesy Ramén Valves)

Ramén Valves, Bromma, Sweden, is using Additive Manufacturing to build a range of industrial control valves from titanium Ti-6Al-4V (Grade 5). The components are produced at AIM Sweden AB, based in Frösön, utilising Electron Beam Powder Bed Fusion (PBF-EB) technology.

The use of AM has allowed Ramén Valves to deliver valves such as the Ramén Ball Sector (shown below) within four weeks from receiving the order, regardless of dimension, shortening the timeline of other traditional methods which can take up to a couple of months. The company also highlighted the sustainability and shortened design time as key benefits when adopting Additive Manufacturing.

The Ramén Ball Sector valve can be manufactured within four weeks from order (Courtesy Ramén Valves)
The Ramén Ball Sector valve can be manufactured within four weeks from order (Courtesy Ramén Valves)

Ramén Ball Sector Valves are used as isolating and control valves for fluids, gases, turbid media and sludge, especially in the mining industry, pulp and paper industry and chemical industry. Abrasive slurries of iron ore, coal, lime and fly ash are also controlled with this type of valve.

“We are proud to be at the forefront when it comes to the development and production of valves using Additive Manufacturing,” the company stated.

www.ramenvalves.com

www.aimsweden.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
February 16, 2023

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap