Titomic to aid development of cold spray AM standards

ApplicationsNews
February 9, 2023
Alongside SAE, Titomic will develop specifications for cold spray 3D printing (Titomic)
Alongside SAE, Titomic will develop specifications for cold spray Additive Manufacturing (Titomic)

Titomic Limited, Brisbane, Australia, has been approved as a sponsor for the development of SAE Cold Spray AM Specifications. Once the SAE specifications have been developed and approved, large organisations within defence and aerospace will more easily adopt the technology in their processes, thereby accelerating use of cold spray as a mainstream manufacturing and coatings technology.

Titomic was approached by SAE International in late 2022 to participate in the development of these specifications and the formal acceptance comes following a review of Titomic’s history and achievements in the technology.

Sinter-based Additive Manufacturing: Beyond the hype, towards industrial success

The development of SAE Cold Spray AM Specifications is expected to provide structure and guidance for the use of cold spray technology in various industries. The new standards will also provide a clear framework for cold spray components to be included in various applications, such as aerospace and defence, where the standards will provide confidence and reassurance to stakeholders.

In addition to sponsoring the specifications, Titomic participates in the SAE AMS-AM Metals and Repair Subcommittee, which is formulating a strategy and road map for SAE AM specifications. The subcommittee has stated that it considers Titomic’s input to be invaluable for this effort.

“We are honoured to be a part of this programme and consider our participation in the development of these specifications a great opportunity to assist the cold spray industry and create a platform for growth and support,” stated Dominic Parsonson, Titomic. “Being invited to contribute in these standards also provide recognition for Titomic as a global leader in cold spray.”

SAE International, formerly known as the Society of Automotive Engineers, is a professional association and standards-developing organisation for engineering professionals in various industries, including Additive Manufacturing.

www.sae.org

www.titomic.com

GET THIS ISSUE:  PDF  |  VIEW ONLINE  |  BUYER’S GUIDE
ApplicationsNews
February 9, 2023

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap