Researchers create digital twin to optimise DED repair process

The paper’s research team aimed to demonstrate how Directed Energy Deposition (DED) 3D printing is superior to other AM repair methods (Courtesy Masayuki Arai/TUS)
The paper’s research team aimed to demonstrate how Directed Energy Deposition is superior to other AM repair methods (Courtesy Masayuki Arai/TUS)

Researchers from Japan’s Tokyo University of Science (TUS) and Suwa University of Science, Nagano, have collaborated with Tocalo Co Ltd, Kobe, to publish a paper in Journal of Thermal Spray Technology outlining a numerical processing analysis system that automatically determines optimum forming conditions in Directed Energy Deposition (DED) Additive Manufacturing.

While DED helps overcome waste when repairing damaged parts compared to traditional Additive Manufacturing, the optimum forming conditions for DED are often a result of trial and error, the team explains. The developed numerical method is reported to automatically generate metal powder deposition elements and predict process forming conditions, temperature distribution, deformation state and residual stress distribution, in advance.

“The thermal radiation-thermal conduction model and the viscoplastic-thermoplastic constitutive model are applied to the stacked elements that constitute the deposited region, so that a wide range of state changes from melting to solidification of the deposited layer of metal powder can be faithfully simulated,” stated Professor Masayuki Arai, TUS. “By incorporating these models into a finite element analysis program, we have developed a new machining analysis system that has never been used before.”

The team numerically simulated the restoration process, and thus, predicted the forming process conditions, temperature distribution, deformation state, and residual stress distribution in advance and verified the findings through experiments. The research showed that the residual stresses in the deposited layer were much lower than those obtained via conventional repair processes.

This DED numerical analysis system is a digital twin of the existing core machining technology based on the fusion of metal in the area to be repaired. The numerical analysis method developed here could be further applied to various industrial applications, such as planning the repair of cavitation thinning on the surface of a blade used in power plant’s circulating pump and devising a method for reducing residual deformation after repairing the thinning of the tip of a gas turbine’s rotor blade.

Together, automation and the prediction of process conditions by the numerical machining analysis system is hoped to make by metal Additive Manufacturing repair by Directed Energy Deposition more effective and sustainable.

“Three-Dimensional Numerical Simulation of Repairing Process by Laser Direct Energy Deposition” is available here.

www.tus.ac.jp

www.sus.ac.jp

www.tocalo.co.jp

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap