Headmade launches M2 tool steel for ColdMetalFusion

Headmade Materials GmbH, Unterpleichfeld, Germany, has announced it is expanding its portfolio of available materials for the ColdMetalFusion standard with the release of its new M2 tool steel material. Developed by Headmade, the M2 tool steel material is said to exhibit well-balanced toughness, wear resistance and hardness properties, as well as part density of up to 99%.

The M2 tool steel is a hardenable high-speed steel with a tungsten-molybdenum matrix suitable for a broad variety of applications and widely used for cutting tools such as twist drills, taps, milling cutters, saws and knives. Worldwide, the M2 type is reputedly the most popular high-speed steel, having replaced grade T1 in most applications. The reasons for this are the materials’ wide heat-treating range as well as the excellent combination of properties.

Headmade Materials was running the material in its pre-series programme for advanced application development. After successful testing in the wake of a lead project for a cutting tool holder with ColdMetalFusion Alliance partner MIMplus, the company is now launching the M2 tool steel as a commercially available material.

Headmade Materials intends to showcase this tool steel together with the already running commercial application at the booth of the ColdMetalFusion Alliance in hall 11.1 booth D48 during Formnext in Frankfurt, Germany.

www.headmade-materials.de

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap