Monash University researchers create high-strength titanium alloy using Additive Manufacturing

Nanotwinned α-precipitates in the PBF-LB microstructure after post-heat treatment at 480°C/6h (Courtesy Professor Huang, Aijung and Dr Zhu, Yuman, et al, ‘Ultrastrong nanotwinned titanium alloys through additive manufacturing)
Nanotwinned α-precipitates in the PBF-LB microstructure after post-heat treatment at 480°C/6h (Courtesy Professor Huang, Aijung and Dr Zhu, Yuman, et al, ‘Ultrastrong nanotwinned titanium alloys through additive manufacturing)

Researchers from Monash University, based in Melbourne, Australia, have published a study which demonstrates the use of Additive Manufacturing to develop an ultra-strong titanium alloy via the manipulation of its microstructure. The research, published in Nature Materials, was done on commercially available material.

The researchers used Laser Beam Powder Bed Fusion (PBF-LB) to manufacture from ß-titanium alloy powders, exploiting the inherent thermal cycling and rapid cooling Additive Manufacturing to achieve a nanoprecipitation microstructure that the researchers believe is a first of its kind.

The additively manufactured parts were subjected to heat treatments at two different temperatures (480 and 520ºC); the tensile stress-strain curves of as-built and post-processed parts were measured. From the curves, the thermally treated samples showed what the researchers called an unexpectedly high level of strength, with a 50–70% relative improvement over the as-built sample. In particular, the UTS after the 480°C post-heat treatment reached the level of 1,611 MPa whilst maintaining a good uniform elongation of 5.4%.

“Titanium alloys require complex casting and thermomechanical processing to achieve the high strengths required for some critical applications,” stated Professor Aijun Huang. “We have discovered that Additive Manufacturing can exploit its unique manufacturing process to create ultra-strong and thermally stable parts in commercial titanium alloys, which may be directly implemented in service.”

He continued, “After a simple post-heat treatment on a commercial titanium alloy, adequate elongation and tensile strengths over 1,600 MPa are achieved – the highest specific strength among all 3D printed metal to date. This work paves the way to fabricate structural materials with unique microstructures and excellent properties for broad applications.”

The process is said to offer a new approach to precipitation strengthening commercial titanium alloys which will enable them to be used in load-bearing applications, making them well suited to aerospace, space, defence, energy and biomedical industries.

‘Ultrastrong nanotwinned titanium alloys through additive manufacturing’ was led by Professor Huang and Dr Yuman Zhu alongside Kun Zhang, Zhichao Meng, Kai Zhang, Peter Hodgson, Nick Birbilis, Matthew Weyland, Hamish L Fraser, Samuel Chao Voon Lim, Huizhi Peng, Rui Yang and Hao Wang. The paper is available here, in full.

www.monash.edu

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap