Tsunami Medical launches AM interbody lumbar implant

The Ustica was developed after years of research, evolving from Tsunami Medical’s first generation TLIF cages (Courtesy Tsunami Medical)

Tsunami Medical, Modena, Italy, a manufacturing company focusing on technological innovation for spinal surgery and diagnostic invasive procedures, has launched Ustica, an additively manufactured titanium transforaminal lumbar interbody fusion (TLIF) cage. This solution has evolved after years of research from the clinically-proven First Generation TLIF cage.

“This new solution meets with the standards of successfully proven Bone InGrowth Technology®,” stated Stefano Caselli, CEO, Tsunami Medical. “Ustica has a unique multi-direction extension mechanism, which allows cranial-caudal height extension in combination with amendment to the required lordosis angle by individual extension in anterior and posterior direction.”

Founded in 1997, Tsunami Medical manufactured invasive diagnostic devices as a subcontractor of large manufacturing companies. In 2010, the company started designing and producing device using Laser Beam Powder Bed Fusion (PBF-LB) Additive Manufacturing technology, resulting in its currently available implant product portfolio.

Peter Witke, CCO, Tsunami Medical, commented, “Solutions with expansion feature show excellent stability characteristics and the cages are printed in one step. Extension of height plus the amendment to lordosis angle, are performed with the same introduction instrument.”

Caselli concluded, “We consider these meaningful extensions of our TLIF cage family, meeting with international market needs and tender requirements.”

www.tsunamimedical.com

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap