ASM’s titanium powder approved for Additive Manufacturing

A 20kg titanium metal ingot produced by ASM (left) and Ti AM parts produced by HANA AMT (Courtesy ASM)

Korean Additive Manufacturing group, HANA AMT, Cheongju, Korea, is reported to have performed a detailed analysis of titanium powder supplied by Australia Strategic Materials (ASM)’s, headquartered in Burswood, Australia, confirming a purity of 99.918% and its suitability for metal Additive Manufacturing.

The test 20kg of titanium powder was produced from a 75 kg run at ASM’s metallisation pilot plant in January 2021. ASM and HANA AMT signed a non-disclosure agreement (NDA) as they progress their negotiations towards an initial 1,500 tonne-per-year off-take agreement for titanium powder.

“This independent review of ASM’s titanium metal powder is a great validation of our patented metal process, confirming the high purity and the environmental benefits of the metal ASM can produce for the manufacturing sector in Korea,” stated David Woodall, ASM Managing Director. “We look forward to progressing negotiations and continuing discussions with other potential off-take and strategic partners during our time in Korea.”

“This is a promising start of the year, with 2021 a foundation year for ASM, as we progress our vision to become a fully integrated critical metals producer – supplying metals from the mine direct to manufacturers, through the delivery of the Dubbo Project and the establishment of our metals business,” continued Woodall.

SEM Image of ASM’s Ti powder (Courtesy ASM)

ASM’s metals business is founded on a novel metallisation process that converts oxides into high purity metals, alloys, and powders using less energy than conventional methods. The pilot plant in South Korea has proven the commercial scalability of the process and is reported to have successfully produced a range of high-purity metals and alloys, including titanium, neodymium, praseodymium, dysprosium, and zirconium.

www.asm-au.com

www.hanaamt.com

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap