BASF’s Forward AM launches Ultrafuse 17-4 PH filament for metal AM applications

The new metal filament Ultrafuse 17-4 PH (Courtesy Forward AM)

Forward AM, an Additive Manufacturing solutions brand of BASF 3D Printing Solutions GmbH, headquartered in Heidelberg, Germany, has launched Ultrafuse® 17-4 PH for the Material Extrusion (MEX)-based Additive Manufacturing process Fused Filament Fabrication (FFF). The new filament, combining stainless steel powder with a polymer binder, compliments the company’s existing Ultrafuse 316L filament range.

Offering high mechanical strength and hardness, the new AM filament is said to be ideally suited for a wide range of applications, such as tooling, jigs and fixtures, and functional prototypes states Forward AM. Good corrosion resistance and the ability to be fully heat treated to high levels of strength and hardness make Ultrafuse 17-4 PH a suitable choice for a range of industries including petrochemicals, aerospace, automotive, and medical, it added.

Ultrafuse metal filaments are specifically developed to work on all common open source FFF machines, from beginner to industrial level, which the company notes makes it one of the easiest and most cost-effective technologies in metal Additive Manufacturing. In 2019, Forward AM launched the company’s first metal filament with Ultrafuse 316L.

“Ultrafuse 17-4 PH is an outstanding result of our strong R&D commitment,” commented Firat Hizal, Head of Metal Systems Group, BASF 3D Printing Solutions. “We filamented more than ten different metals from titanium to tool-grade steels, and several alternative materials to print support structures within this year. Going forward we will continue to introduce the new filaments that the market and our customers demand.”

Hizal added, “We have already established a distribution network that collaborates closely with our debinding and sintering service partners in different regions and can thus deliver an integrated end-to-end solution. We are proud to extend our portfolio with Ultrafuse 17-4 PH.”

www.forward-am.com

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap