Poly-Shape and Constellium to explore aluminium Additive Manufacturing

A research team is working to develop innovative additively manufactured components from aluminium powders (Courtesy P Urvoy/Poly-Shape)

Poly-Shape, an AddUp company, has signed a contract with Constellium, Paris, France, to research and develop innovative components made from aluminium powder. The components will be additively manufactured from the Aheadd® powders recently developed by Constellium.

“This is the result of the flexibility of our structures, our reactivity and the high quality of our teams, in particular the research and development sector,” stated Stephane Abed, CEO of Poly-Shape. “From the beginning, our strong culture of R&D places innovation at the centre of the company, to meet the expectations of the demanding high-tech industries in which we operate.”

With experience as a provider of metal Additive Manufacturing services for industries such as aeronautical, motorsports and energy, Poly-Shape has an in-house R&D department and participates in numerous multinational industrial innovation projects. This includes projects to develop emerging processes to validate new materials and new design methods, improve manufacturing parameters for existing machines, and perform testing of future machines.

The new collaboration is reported to be fully integrated into the overall Addup R&D policy, which includes a joint-venture between France’s Michelin and Fives.

www.poly-shape.com

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap