Optomec expands capabilities with aluminium AM using LENS DED

Optomec’s LENS DED system additively manufacturing aluminium powder onto an aluminium substrate (Courtesy Optomec)

Optomec, headquartered in Albuquerque, New Mexico, USA, has announced an advancement in capability for its LENS Directed Energy Deposition (DED) Additive Manufacturing machines and the repair of aluminium alloys. The advancement reportedly enables LENS DED machines to be used to deposit any aluminium alloy, including those developed specifically for their improved properties for AM processing.  

This development helps open up the transportation and aerospace industries to Additive Manufacturing and the repair of complex aluminium alloy parts using powder-based DED. Additionally, the use of Optomec’s LENS simultaneous 5-axis system is said to enable the processing of aluminium alloy parts with complex geometries without the need for support structures. The company explains that the deposition of aluminium alloys in a controlled atmosphere glove-box with very low levels of oxygen and moisture ensures the achievement of components with superior mechanical properties.

David Otazu, LENS Applications Engineer at Optomec, commented, “Our engineers have developed process parameters for aluminium alloys to provide an excellent surface finish, high deposition rates and a density of ~99.9%.” 

With this advancement, the company believes that its Optomec LENS systems can now successfully process all common materials used for Additive Manufacturing, which as well as aluminium include steels, titanium, nickel and copper.

www.optomec.com

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap