Indo-MIM accelerates move to offer metal Binder Jetting AM

News
December 13, 2019
Indo-MIM accelerates move to offer metal Binder Jetting AM
Indo-MIM will accept prototype orders from January 2020 (Courtesy Indo-MIM)

Indo-MIM, a leading global manufacturer of components by Metal Injection Moulding (MIM), headquartered in Bangalore, India, reports that from January 2020 it will be accepting prototype sample orders for metal AM parts. Orders are expected to be produced on the company’s Desktop Metal Production System at its facility in San Antonio, Texas, USA.

Indo-MIM is initially offering customers two material choices, 17-4 PH and 316L stainless steels, with more material options to be added by summer 2020. Suitable part weight is said to be between 5–250 g, and prototype samples are available within ten days. Series production volumes are reported to be in the range of 10–50,000 parts per year, with the company saying it will offer increased volumes of up to 500,000 parts per year by 2021.

Indo-MIM has MIM production facilities in both India and the USA, as well as further sales offices in Europe and Asia.

www.indo-mim.com

News
December 13, 2019

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap