Betatype & nTopology develop optimised rocket nozzle part by metal AM

News
July 19, 2019
The metal additively manufactured, functionally optimised rocket nozzle part, developed by nTopology and Betatype (Courtesy Betatype)

Betatype, London, UK, and nTopology, New York City, USA, recently partnered to develop and produce a functionally optimised rocket nozzle part by metal Additive Manufacturing. The project is said to have resulted in a notable reduction in build time on the AM system, from twenty-five to eighteen hours. 

nTopology designed the base mechanical structure of the part using its nTop Platform software to convert a 3D model of the nozzle part into an implicit model. The team then used nTopology’s topology optimisation and simulation tools to optimise the design of the part for the Laser Powder Bed Fusion (L-PBF) process, using Betatype’s unique Engine and Process Control technology 

The part was additively manufactured in titanium on a Renishaw RenAM250 system by Betatype. Designed to serve as a test part, it highlights how functionality can be improved through the application of intelligent design while still ensuring a part is fit for purpose, and that complexity and functionality does not necessarily come at the expense of productivity. 

Sarat Babu, Betatype’s Founder and CEO, stated, “Betatype’s partnership with nTopology is an excellent demonstration of how we can work with talented designers to make Additive Manufacturing perform. The application clearly shows the benefits of combining the functional design and optimisation skills of our partner with process optimisation through our technology to achieve productivity levels that would not otherwise be possible with a standard metal L-PBF platform.”

Brad Rothenberg, Founder and CEO of nTopology, added, “For serial production in Additive Manufacturing to work, it must make business sense. Through the partnership between nTopology and Betatype, and our shared belief in solving engineering problems by linking design, simulation, and manufacturing processes directly, we are able to present a strong business case for Additive Manufacturing. We enable our customers to design and manufacture complex parts with speed, efficiency and reliability. We could not be happier with the results of this rocket nozzle case study and are looking forward to working on more joint projects.”

www.betaty.pe 

www.ntopology.com 

News
July 19, 2019

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap