Metallic Advanced Materials for Aeronautics project coupling traditional metallurgy with wire-fed metal AM

News
July 2, 2019

A 116 cm diameter dome for a satellite fuel tank produced on a Sciaky EBAM 110 machine, pictured here at Lockheed Martin’s space facility in Denver, Colorado, USA (Courtesy Lockheed Martin)

 

Sciaky, Inc., a subsidiary of Phillips Service Industries, Inc. (PSI), headquartered in Chicago, Illinois, USA, has entered into an R&D initiative with Aubert & Duval, Paris, France, and Airbus, headquartered in Leiden, the Netherlands, driven by the Saint Exupéry Institute for Research in Technology (IRT), Toulouse, France. The Production Engineering laboratory of the National School of Engineering in Tarbes, France will serve as an academic partner for this project, which is titled Metallic Advanced Materials for Aeronautics (MAMA).

The goal of the project is to couple traditional metallurgy (high-power closed die forging) with wire-fed metal AM (in this case, Sciaky’s Electron Beam Additive Manufacturing (EBAM®) process) to develop new manufacturing processes for titanium alloy aircraft parts. In its first phase, the project has a global funding of €4.2 million (just under $4.8 million), of which 50% comes from the French State as part of its ‘Investing in the Future’ programme, and the other 50% from industrial partners.

Scott Phillips, President and CEO of Sciaky, Inc., stated, “Sciaky is proud to work with the Saint Exupéry IRT, Aubert & Duval and Airbus on this exciting project. Industrial metal Additive Manufacturing technology continues to break new ground every day, and Sciaky is committed to keeping EBAM at the forefront of this movement.”

www.sciaky.com

www.aubertduval.com

www.airbus.com

www.irt-saintexupery.com

News
July 2, 2019

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap