Titomic to additively manufacture extruder technology parts for C.A.Picard

News
July 1, 2019

Titomic Limited, Melbourne, Australia, has entered into an agreement with plastic extruder parts manufacturer C.A.Picard Group, Remscheid, Germany, to produce metal parts for the extruder technology market. Titomic will use its proprietary Kinetic Fusion™ Additive Manufacturing process to build a hardened metal extrusion screw, with the aim of reducing the current cost and testing potential improvements in wear resistance.

On the successful completion of prototype test trials by C.A.Picard, Titomic stated it will negotiate a contract to supply production from its TKF Melbourne Bureau for single, twin, and multi-screw extrusion systems. These parts currently developed by C.A.Picard are distributed to over fifty countries, with the major markets being Europe, Asia, America and the Far East. The global plastic extrusion machine market reportedly generated $6.05 billion in 2017, and is expected to reach $8.24 billion by 2025, growing at a CAGR of 3.8% from 2018–2025.

Jeff Lang, Titomic’s Managing Director, commented, “Titomic’s partnering with C.A.Picard to additively manufacture their extrusion screw products showcases the unique capability of Titomic Kinetic Fusion to utilise tooling steels to be cost competitive against traditional metal manufacturing processes. We believe that by partnering with visionary industry leaders like C.A.Picard, Titomic can improve the efficiency of metal manufacturing and mechanical performance properties, providing real commercial benefits to our customers.

Michael Busenbecker, Global Head of Research and Development, C.A.Picard, stated, “We are committed to producing the best quality parts for the extruder market and are pleased to be working with Titomic to bring their state of the art Titomic Kinetic Fusion Process on board. We believe that the future lies in finding efficiency without compromising on value and quality and we look forward to working with Titomic on this project.”

www.titomic.com

www.capicard.de

News
July 1, 2019

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap