Additec launches desktop metal Additive Manufacturing system

News
January 22, 2019
Additec launches desktop metal Additive Manufacturing system

Additec’s desktop μPrinter offers a build volume of 120 x 160 x 450 mm (Courtesy Additec)

 

Additec, located in Las Vegas, USA and Bremen, Germany, has launched a new desktop-size metal AM system named the μPrinter. The μPrinter can processes both wire and powder feedstock using the company’s unique Laser Metal Deposition-Wire Powder (LMD-WP) process, with the complete system being offered at a price point starting at $90,000 USD.

Producing parts from wire has the advantage of low material cost and high availability of stock, being safe and clean to handle. Combining the ability to process powder is said to close the gap to conventional LMD, whilst also allowing users to mix alloys in-situ. Switching between wire and powder on the μPrinter does not require a nozzle change and can be done automatically on the same part.

Additec’s LMD-WP process works by having multiple high-power diode laser sources arranged around the central axis of the deposition head. Wire is fed through a central wire guide, while powder is fed through an annular gap nozzle around the wire guide. Closed loop process control is a standard feature on the μPrinter, with the system being controlled either via a locally hosted web interface, or through USB.

“Process stability was the most important aspect for the development of the μPrinter. Because wire based coaxial deposition is not as common as powder LMD, we developed our own process control structure, that not only adjusts the processing parameters on the fly, but also measures the height of the individual layers, and adjusts nozzle to part distance automatically,” the company stated.

The print envelope is reported to be 120 x 160 x 450 mm (XYZ), and in addition to Additive Manufacturing, it is also suitable for cladding and repair work on small components.
Additec’s LMD-WP process, launched in 2016, is also offered as a retrofit package that could be used to turn existing CNC platforms into metal AM or hybrid manufacturing systems.

www.additec.net/μPrinter

News
January 22, 2019

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap