Sciaky to deliver hybrid EBAM system to aerospace parts manufacturer

An Electron Beam Additive Manufacturing system produced by Sciaky (Courtesy Sciaky, Inc.)

 

Sciaky, Inc., Chicago, Illinois, USA, a subsidiary of Phillips Service Industries, Inc. (PSI), states that a “prominent Southeast Asian aerospace parts manufacturer” has purchased a dual-purpose Electron Beam Additive Manufacturing (EBAM®) and EB Welding System. The hybrid machine, which is reported to be the only one of its kind, will be customised with special controls to switch from AM to welding quickly and easily.

The aerospace parts manufacturer will use the system to additively manufacture metal structures, as well as weld dissimilar materials and refractory alloys for these structures and other aerospace parts. Delivery of the system is scheduled for the second quarter of 2019.

“Sciaky is excited to work with this innovative company,” stated Scott Phillips, President and CEO of Sciaky, Inc. “This strategic vision will allow this manufacturer to reduce operating costs by combining two industry-leading technologies into a single turnkey solution. No other metal 3D printing supplier can offer this kind of game-changing capability.”

Sciaky’s EBAM systems can be used to produce parts ranging from 203 mm (8 in) to 5.79 m (19 ft) in length. EBAM is also reported to be the fastest deposition process in the metal AM market, with gross deposition rates ranging from 3.18-11.34 kg (7-25 lbs) of metal per hour.

Sciaky’s systems also incorporate IRISS® (Interlayer Real-time Imaging and Sensing System), a real-time adaptive control system that can sense and digitally self-adjust metal deposition with precision and repeatability. According to Sciaky, this innovative closed-loop control is the primary reason that its systems are able to deliver consistent part geometry, mechanical properties, microstructure and metal chemistry.

Sciaky’s EB Welding Systems are able to meet rigid military specifications for the manufacturing of items such as airframes, landing gear, jet engines, guided missiles and vehicle parts. They incorporate an internal moving EB welding gun with multi-axis motion, providing beam access for unusual joint configurations.

www.sciaky.com

News
October 17, 2018

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap