Metal Additive Manufacturing of structures “smaller than a speck of dust”

News
February 19, 2018
Metal Additive Manufacturing of structures “smaller than a speck of dust”

The final metal additively manufactured nanostructure was reported to be smaller than a speck of dust (Courtesy Caltech)

 

A group of scientists at the California Institute of Technology (Caltech), California, USA, have reportedly developed a new process which enables the metal Additive Manufacturing of structures smaller than a human hair and invisible to the naked eye. In a paper published in Nature Communications, ‘Additive Manufacturing of 3D Nano-Architected Metals’, the group stated that the process could be scaled up for use in a wide variety of applications, including the production of tiny medical implants, ultralightweight aircraft components 3D logic circuits on computer chips.

The principal researchers on the project were Julia Greer, Professor of Materials Science, Mechanics and Medical Engineering at Caltech’s Division of Engineering and Applied Science, and graduate student Andrey Vyatskikh. While Greer has previously additively manufactured nanostructures from materials such as ceramics, polymers and organic compounds, this is the first time the team has successfully applied her nanoscale AM technique to metals.

Greer’s process works by lasing a liquid or resin in specific locations with just two photons, in a process called ‘two-photon lithography’. This generates enough energy to harden liquid polymers into solids, but is not strong enough to fuse metal. “Metals don’t respond to light in the same way as the polymer resins that we use to manufacture structures at the nanoscale,” explained Greer. “There’s a chemical reaction that gets triggered when light interacts with a polymer that enables it to harden and then form into a particular shape. In a metal, this process is fundamentally impossible.”

The solution, developed by Vyatskikh, is to use organic ligands (molecules with the ability to bind to trace metals in the aquatic dissolved phase) to create a resin comprising primarily of polymer, but ‘carrying with it’ a metal which can then be additively manufactured. Vyatskikh’s technique bonds nickel with organic molecules to create a liquid ‘syrup’ which was then lased with a two-photon laser to build a structure according to a CAD design.

Under the laser, the organic molecules hardened into ‘building blocks’ for the structure, which the nickel atoms were incorporated into. The result was an additively manufactured nanostructure comprising a blend of metal ions and nonmetal organic molecules.

Vyatskikh then heated the nanostructure slowly in a vacuum to 1000°C – below the melting point of nickel, but hot enough to vaporise the organic materials in the structure and leave only the metal. This heating process also resulted in fusing of the metal particles, as well as structural shrinkage of about 80%. The combination of Greer’s nanoscale AM process and the part shrinkage resulted in a final structure which was reported to be smaller than a speck of dust.

“In the structure we built for the paper, the diameter of the metal beams in the printed part is roughly 1/1000th the size of the tip of a sewing needle,” stated Vyatskikh. Greer and Vyatskikh report that the process requires some refinement, with the initial structures showing some voids left behind by the vaporised organic material as well as some minor impurities. The process also requires scaling up to be suitable for many of its planned applications.

The research team stated that it is interested in expanding adapting the process to work with other metals, such as tungsten and titanium, which are challenging to produce at very small scales. Co-authors on the paper include Akira Kudo, Caltech Resnick Sustainability Institute postdoctoral scholar in Applied Physics and Materials Science, Carlos Portela, graduate student in Mechanical Engineering, Stéphane Delalande, of the Centre Technique de Vélizy, France, and Xuan Zhang of Tsinghua University, China. Research funding was provided by the US Department of Defense.

www.caltech.edu

News
February 19, 2018

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap