Metal AM engine part completes maiden flight on Finnish fighter jet

News
February 4, 2018
Metal 3D printed engine part completes maiden flight on Finnish fighter jet

The part, developed by Patria, was installed on an F/A-18 Hornet fighter operated by the Finnish airforce (Courtesy Finnish Air Force)

 

Finland’s first metal additively manufactured aircraft engine part has completed its maiden flight. The part, developed by Patria, was installed on an F/A-18 Hornet fighter operated by the Finnish airforce and flew for the first time on January 5, 2018.

Full details of the part have not been disclosed, however Patria reports that it was additively manufactured from Inconel 625 superalloy. The engine part was designed in accordance with Military Design Organisation Approval (MDOA), meeting European Military Aviation Requirements (EMARs) and granted by the Finnish Military Aviation Authority (FMAA).

Ville Ahonen, Vice President of Patria’s Aviation business unit, stated, “For this part, the development work has been done over the last two years, with the aim of exploring the manufacturing process for 3D printable parts, from drawing board to practical application.”

“Using 3D printing to make parts enables a faster process from customer need to finished product, as well as the creation of newer, better structures. We will continue research on additive manufacturing methods, with the aim of making the new technology more efficient,” he concluded.

www.patria.fi

News
February 4, 2018

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap