German Additive Manufacturing company receives FDA clearance to supply spinal cages to US market

News
January 19, 2018
German Additive Manufacturing company receives FDA clearance to supply spinal cages to US market

EIT’s metal AM spinal cages for TLIF (pictured left) and ALIF (pictured right) procedures (Courtesy EIT)

 

Emerging Implant Technologies GmbH (EIT), a German medical device maker focused exclusively on additively manufactured technologies for spinal application, reports that it has received full 510(k) approval from the US Food and Drug Administration (FDA) for its metal AM spinal cages. EIT offers a number of spinal products suitable for ALIF (Anterior Lumbar Interbody Fusion), TLIF (Transforaminal Lumbar Interbody Fusion), PLIF (Posterior Lumbar Interbody Fusion) and Cervical procedures.

The implants combine an osteo-influential scaffold with designs which address spinal alignment, and are produced in EIT Cellular Titanium®, a porous titanium structure designed according to research on the ideal pore shape and size to optimise osseointegration (bone in-growth). Each implant combines an osteo-influential scaffold with designs to address spinal alignment.

All of the company’s implants are produced using Selective Laser Melting, and are said to have been subject to a number of clinical case studies which demonstrate extensive bone in-growth in a short time frame. They have been used in over 10,000 cases in over fifteen countries including Germany, France, Australia, Korea and the Netherlands. Following the 510(k) approval, EIT stated it is moving towards full commercialisation.

Guntmar Eisen, EIT Co-Founder and CEO, stated, “This is a major milestone for EIT. We look forward to bringing our unique technologies to the United States and partnering with top-tier surgeons and institutions to bring the best results to patients that are in need of these devices.”

www.eit-spine.de

News
January 19, 2018

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap