CDU boosts metal Additive Manufacturing in Australia with purchase of LightSPEE3D Printer

News
July 20, 2017
Charles Darwin University boosts metal Additive Manufacturing in Australia with purchase of LightSPEE3D Printer

The LightSPEE3D Printer (Courtesy SPEE3D)

Charles Darwin University (CDU), Darwin, Australia, has announced that it will acquire a LightSPEE3D Printer from Darwin-based Additive Manufacturing start-up SPEE3D. The acquisition will be made possible by a grant of AUD $400,000 from Australia’s Northern Territories Government, which hopes to drive innovation in the region by boosting AM development.

The LightSPEE3D AM system, developed by SPEE3D’s Steven Camilleri, is based on cold spray technology and reportedly enables metal Additive Manufacturing at speeds of up to 1000 x faster than those allowed by existing powder bed fusion and wire based AM. SPEE3D claims that the machine has the potential to transform industrial metal Additive Manufacturing.

Michael Gunner, Chief Minister for the Northern Territory, stated that the printer would form the centrepiece of a new industrial research hub to be based at CDU’s Casuarina campus. This hub, the Minister stated, will pave the way for the creation of jobs into the future for Territorians as well as generating new economic opportunities in the region.

“We want to partner with local enterprises to drive innovation here in the Territory. By diversifying the economy through innovation we are opening the door to new economic opportunities for Territorians – both now and into the future,” he commented.

Together with CDU, SPEE3D has formed the Advanced Manufacturing Alliance (AMA) based at Casuarina campus. CDU’s Professor Maddocks stated the AMA also would work to develop applications for the use of the new technology in remote areas, with the aim of improving supply chains and lowering operating costs.

www.cdu.edu.au

www.spee3d.com

News
July 20, 2017

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap