GKN Sinter Metals begins automotive series production of metal AM components

Team GKN and Additive Industries (© GKN Sinter Metals/Photographer/Ralf Bille)

 

GKN Sinter Metals has announced it has begun series production of additively manufactured precision automotive parts at its plant in Radevormwald, Germany. The company is using its MetalFAB1 system from Additive Industries to produce complex engine and transmission components for the original equipment and replacement parts markets. Customers are said to include most of the leading automakers and their system suppliers.

The MetalFAB1 can simultaneously print hundreds of parts on a single build plate. “Depending on how many data sets we feed into the MetalFAB1, these can be 300 identical or 300 different parts. This gives us unprecedented production capacity and flexibility,” stated Dr Simon Hoeges, GKN AM Director.

 

GKN Sinter Metals begins automotive series production of metal AM components

Simon Hoeges, GKN AM Director, in front of the MetalFAB1 (© GKN Sinter Metals/Photographer/Ralf Bille)

 

In addition to the AM build process, the MetalFAB1 also incorporates stress relief heat treatment and automated handling. The system uses powder bed fusion with multiple lasers. In a joint development programme the technology is further optimised for the needs of the automotive industry.

GKN Sinter Metals is the world’s largest producer of precision powder metal products, the company offers extensive technical expertise in design, testing and various process technologies. GKN Sinter Metals offers a full range of complex shapes and high-strength products for automotive, industrial and consumer markets worldwide. With the MetalFAB1 system, GKN Sinter Metals stated that it is in a position to offer its customers around the world a range of complex and creative product solutions in next to no time.

www.gknsintermetals.com

News
November 14, 2016

TRUSTED CONTENT. TARGETED AUDIENCE

Advertise with Metal AM and access a global base of 50,000+ AM professionals.

Contact Jon Craxford: [email protected]

Request a Media Pack
  • AM machines
  • Process monitoring & calibration
  • Heat treatment & sintering
  • HIP systems & services
  • Pre- & post-processing technology
  • Powders, powder production and analysis
  • Part manufacturers
  • Consulting, training & market data

Don’t miss a thing – register for our newsletter

Don't miss any new issue of Metal AM magazine, and get the latest industry news. Sign up to our twice weekly newsletter.

Register now

Join 40,000+ other AM professionals – follow us online

About Metal Additive Manufacturing magazine

Metal AM magazine, published quarterly in digital and print formats, is read by a rapidly expanding international audience.

Our audience includes component manufacturers, end-users, materials and equipment suppliers, analysts, researchers and more.

In addition to providing extensive industry news coverage, Metal AM magazine is known for exclusive, in-depth articles and technical reports.

Our focus is the entire metal AM process from design to application.

Each issue is available as an easy-to-navigate digital edition and a high-quality print publication.

Discover our magazine archive…

The free to access Metal Additive Manufacturing magazine archive offers unparalleled insight into the world of metal Additive Manufacturing from a commercial and technological perspective through:

  • Reports on visits to leading metal AM part manufacturers and industry suppliers
  • Articles on technology and application trends
  • Information on materials developments
  • Reviews of key technical presentations from the international conference circuit
  • International industry news

All past issues are available to download as free PDFs or view in your browser.

Browse the archive

Share via
Copy link
Powered by Social Snap